Sulphuric acid anodising Inspection and Quality Checks
A quality check on completed parts after they have left the anodising line needs to mean something. The following describes what actual quality control for anodizing looks like.
Visual Inspection Under Controlled Lighting
A visual inspection of the anodising finish is carried out under controlled lighting, which consists of fluorescent or daylight-equivalent tubes. All parts are inspected for any signs of staining or blotching, as well as for burning (darker, possibly powdery patches which occur when current density becomes too high). Also for any powdery or chalky areas, which occur where the seal has failed. A part may measure up within specified limits for thickness but fail due to uneven coloration across the surface of the part, as this would indicate an inconsistent process having been used.
Coating Thickness Measurement
The thickness of the anodic layer needs to be within a specified micron range. This is typically measured using an eddy current gauge pressed against the surface of the workpiece. The layer thickness can also be measured by cutting a cross-section through a sample part and then measuring the anodic layer under a microscope. This needs to be within the specified micron range. It must not be too thin to provide the necessary wear and corrosion resistance and must not be too thick in order to fit other components and to pass thread gauges.
Seal Quality Testing
After anodising has taken place the anodized layer is porous until it is sealed. Sealing must be carried out successfully to prevent the coating absorbing dye, dirt and moisture etc. A simple test to check for good sealing is a dye-stain test. Ink is applied to the surface of the anodized part in the form of a felt tip pen mark. The mark is left to penetrate for a short space of time and then wiped off with a cloth. A well sealed part will wipe clean, a poorly sealed part will show signs of the stain remaining on the surface. An admittance test is an alternative method of checking for good sealing. This test measures the admittance of the surface to a small electrical signal.
Adhesion Checks
A simple test to check for adhesion is the tape test. A piece of tape is pressed onto the coating and then instantly pulled off. If any of the coating comes off with the tape then the part has failed the adhesion test. Coupons processed at the same time as the production parts can also be bent sharply and then examined for any signs of flaking or cracking. Any such failure will have originated from the surface preparation prior to anodising and will be a problem of the aluminium surface prior to anodising rather than a problem with the anodising process itself.
Dimensional Verification

After the anodising process the anodic layer adds to the thickness of the part. Therefore the thickness of the coating must be added to the dimension of the part before it was anodised when measuring critical features such as bores, surface finish and threads. These features must be measured with precision measuring equipment such as thread gauges after the anodising process. A part that was within dimension before anodising could now be out of dimension due to the coating thickness not having been allowed for when machining the part.
Corrosion Resistance Testing
Salt Spray Testing – This test is used to test for corrosion of an anodized surface. The part is placed in a controlled chamber and exposed to a fine salt mist for a specified time (usually 168 hours or 336 hours). The part is then removed from the test chamber and inspected for any signs of corrosion or pitting. This test is normally carried out on coupons, processed as part of the same batch of components, at a UKAS-accredited test laboratory.
Colour and Appearance Matching
Dye anodising parts have to be checked for colour on a visual inspection against approved samples under the same set up of viewing as used for the general surface inspection. Acceptable variation between batches is normally allowed but this has to be stipulated within agreed limits for normal, non-functional items. For cosmetic items or items that are to be used as promotional items then colour can be a very important criteria and needs to be strictly controlled.
Paperwork and Traceability
The last thing to check is the paperwork. Any properly processed batch of anodizing should have full process records for the bath it was anodized in, including its chemistry, temperature and the time it was anodized. This will be accompanied by a process certificate confirming that the part has been anodized to the correct specification and a full Certificate of Conformity detailing what parts have been processed as part of that batch and in which anodizing run they were processed. All of this can provide useful information on the properties of the coating, but more importantly it provides full traceability of all parts processed through the anodizing plant. In addition the anodizing process involves the use of sulphuric acid which is covered under the safe handling of sulphuric acid under the Control of Substances Hazardous to Health (COSHH) regulations and the discharge from the anodizing process is covered by environmental permitting rules for the anodising process. Therefore all traceability of the anodizing process is recorded to provide full proof that a company is operating within the laws for the anodising process.
Simple individual checks are not enough to distinguish between anodised articles that have merely been anodised and those which have been processed in accordance with a written specification. The established chemistry of acid-based surface treatments must be developed into consistent and checkable processes, and this can only be achieved by the systematic checking of every part at every stage.